Gouda Vuurvast CURON 120 C Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 120 C Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
30.0 - 40.0 MPa

@Temperature 100 °C
4350 - 5800 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.480 - 0.580 W/m-K

@Temperature 100 °C
3.33 - 4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.520 - 0.620 W/m-K

@Temperature 600 °C
3.61 - 4.30 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.560 - 0.660 W/m-K

@Temperature 1000 °C
3.89 - 4.58 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Shrinkage -0.100 - 0.500 %

@Temperature 1000 °C
-0.100 - 0.500 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 33 %
33 %
SiO2 50 %
50 %
Descriptive Properties Value Comments
ASTM Classification A
Material Consumption per 1 m3 1900 kg
Mixing Water 13-16 liters