Material Notes:
Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.50 - 2.60 g/cc
0.0903 - 0.0939 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
75.0 - 85.0 MPa

@Temperature 100 °C
10900 - 12300 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.870 - 0.970 W/m-K

@Temperature 100 °C
6.04 - 6.73 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.09 - 1.19 W/m-K

@Temperature 600 °C
7.56 - 8.26 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.22 - 1.32 W/m-K

@Temperature 1000 °C
8.47 - 9.16 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Shrinkage -0.200 - 0.600 %

@Temperature 1000 °C
-0.200 - 0.600 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 39 %
39 %
CaO 40 %
40 %
SiO2 4.0 %
4.0 %
Descriptive Properties Value Comments
ASTM Classification A
Material Consumption per 1 m3 2500 kg
Mixing Water 9-11 liters
per 100 kgs dry material