Material Notes:
Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/holding furnaces and ladles. Due to its unique raw materials, Curon 13 S contains two hydraulic binders and therefore will remain very strong. Curon 13 SC is worldwide used in the aluminum and cement industry.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.50 - 2.60 g/cc
0.0903 - 0.0939 lb/in³
After drying at 110°C
Particle Size <= 10000 µm
<= 10000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
60.0 - 70.0 MPa

@Temperature 100 °C
8700 - 10200 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.780 - 0.880 W/m-K

@Temperature 100 °C
5.41 - 6.11 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.870 - 0.970 W/m-K

@Temperature 600 °C
6.04 - 6.73 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.960 - 1.06 W/m-K

@Temperature 1000 °C
6.66 - 7.36 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Shrinkage -0.150 - 0.150 %

@Temperature 1000 °C
-0.150 - 0.150 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 67 %
67 %
SiO2 3.0 %
3.0 %
Descriptive Properties Value Comments
ASTM Classification B
Material Consumption per 1 m3 2500 kg
Mixing Water 8-10 liters
per 100 kgs dry material