Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 130 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 130 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1200 °C
3630 - 5080 psi

@Temperature 2190 °F
Cold Crushing Strength
30.0 - 40.0 MPa

@Temperature 100 °C
4350 - 5800 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.560 - 0.660 W/m-K

@Temperature 600 °C
3.89 - 4.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.650 - 0.750 W/m-K

@Temperature 1200 °C
4.51 - 5.20 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Shrinkage -1.00 - 0.000 %

@Temperature 1200 °C
-1.00 - 0.000 %

@Temperature 2190 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 35 %
35 %
SiO2 49 %
49 %
Descriptive Properties Value Comments
ASTM Classification B
Material Consumption per 1 m3 1950 kg
Mixing Water 12-15 liters
per 100 kgs dry material
Users viewing this material also viewed the following: