Material Notes:
This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strength over the whole range of temperatures.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Particle Size <= 3000 µm
<= 3000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1300 °C
5080 - 6530 psi

@Temperature 2370 °F
Cold Crushing Strength
45.0 - 55.0 MPa

@Temperature 100 °C
6530 - 7980 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 3.95 - 4.05 W/m-K

@Temperature 100 °C
27.4 - 28.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
4.05 - 4.15 W/m-K

@Temperature 600 °C
28.1 - 28.8 BTU-in/hr-ft²-°F

@Temperature 1110 °F
4.05 - 4.15 W/m-K

@Temperature 1300 °C
28.1 - 28.8 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1400 °C
2550 °F
Shrinkage -0.150 - 0.150 %

@Temperature 1300 °C
-0.150 - 0.150 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 16 %
16 %
SiC 60 %
60 %
SiO2 11 %
11 %
Descriptive Properties Value Comments
ASTM Classification C
Material Consumption per 1 m3 2300 kg
Mixing Water 8-10 liters
per 100 kgs dry material