Material Notes:
Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1300 °C
5080 - 6530 psi

@Temperature 2370 °F
Cold Crushing Strength
45.0 - 55.0 MPa

@Temperature 100 °C
6530 - 7980 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 100 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.600 - 0.700 W/m-K

@Temperature 600 °C
4.16 - 4.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.670 - 0.770 W/m-K

@Temperature 1300 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1300 °C
-0.400 - 0.400 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 45 %
45 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 44 %
44 %
Descriptive Properties Value Comments
ASTM Classification C
Material Consumption per 1 m3 2100 kg
Mixing Water 10-12 liters
per 100 kgs dry material