Material Notes:
Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
After drying at 110°C
Particle Size <= 3000 µm
<= 3000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 10.0 - 20.0 MPa

@Temperature 1300 °C
1450 - 2900 psi

@Temperature 2370 °F
Cold Crushing Strength
20.0 - 30.0 MPa

@Temperature 100 °C
2900 - 4350 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.500 - 0.600 W/m-K

@Temperature 100 °C
3.47 - 4.16 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.550 - 0.650 W/m-K

@Temperature 600 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.640 - 0.740 W/m-K

@Temperature 1300 °C
4.44 - 5.14 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1480 °C
2700 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1300 °C
-0.500 - 0.500 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 43 %
43 %
SiO2 41 %
41 %
Descriptive Properties Value Comments
ASTM Classification D
Material Consumption per 1 m3 1950 kg
Mixing Water 13-16 liters
per 100 kgs dry material