Gouda Vuurvast CURON 145 P Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 145 P Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.80 - 1.90 g/cc
0.0650 - 0.0686 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 7.00 - 13.0 MPa

@Temperature 100 °C
1020 - 1890 psi

@Temperature 212 °F
Cold Crushing Strength
7.00 - 13.0 MPa

@Temperature 1400 °C
1020 - 1890 psi

@Temperature 2550 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.490 - 0.590 W/m-K

@Temperature 600 °C
3.40 - 4.09 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.570 - 0.670 W/m-K

@Temperature 1400 °C
3.96 - 4.65 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
Shrinkage -1.00 - 1.00 %

@Temperature 1400 °C
-1.00 - 1.00 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 53 %
53 %
SiO2 41 %
41 %
Descriptive Properties Value Comments
ASTM Classification C
Material Consumption per 1 m3 1750 kg
Mixing Water 18-22 liters
per 100 kgs dry material