Gouda Vuurvast CURON 150 HS Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 150 HS Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
After drying at 110°C
Particle Size <= 7000 µm
<= 7000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 55.0 - 65.0 MPa

@Temperature 1300 °C
7980 - 9430 psi

@Temperature 2370 °F
Cold Crushing Strength
65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.570 - 0.670 W/m-K

@Temperature 600 °C
3.96 - 4.65 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.670 - 0.770 W/m-K

@Temperature 1300 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1300 °C
-0.500 - 0.500 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 42 %
42 %
Descriptive Properties Value Comments
ASTM Classification D
Material Consumption per 1 m3 2150 kg
Mixing Water 10-12 liters
per 100 kgs dry material