Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
45.0 - 55.0 MPa

@Temperature 100 °C
6530 - 7980 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.490 - 0.590 W/m-K

@Temperature 100 °C
3.40 - 4.09 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.550 - 0.650 W/m-K

@Temperature 600 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.650 - 0.750 W/m-K

@Temperature 1300 °C
4.51 - 5.20 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1300 °C
-0.400 - 0.400 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 42 %
42 %
Descriptive Properties Value Comments
ASTM Classification D
Material Consumption per 1 m3 2150 kg
Users viewing this material also viewed the following: