Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 150 RN Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 150 RN Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.820 - 0.920 W/m-K

@Temperature 600 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.870 - 0.970 W/m-K

@Temperature 1000 °C
6.04 - 6.73 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -0.500 - 1.50 %

@Temperature 1000 °C
-0.500 - 1.50 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 81 %
81 %
Fe2O3 <= 1.0 %
<= 1.0 %
SiO2 8.0 %
8.0 %
Descriptive Properties Value Comments
ASTM Classification D
Material Consumption per 1 m3 2550 kg
Mixing Water 10-12 liters
per 100 kgs dry material