Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 165 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 165 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.25 - 2.35 g/cc
0.0813 - 0.0849 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.610 - 0.710 W/m-K

@Temperature 100 °C
4.23 - 4.93 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.680 - 0.780 W/m-K

@Temperature 600 °C
4.72 - 5.41 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.790 - 0.890 W/m-K

@Temperature 1300 °C
5.48 - 6.18 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage -1.50 - 1.50 %

@Temperature 1300 °C
-1.50 - 1.50 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 62 %
62 %
Fe2O3 1.5 %
1.5 %
SiO2 30 %
30 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2250 kg
Mixing Water 8-10 liters
per 100 kgs dry material
Copyright © lookpolymers.com All Rights Reserved