Material Notes:
Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
50.0 - 60.0 MPa

@Temperature 1300 °C
7250 - 8700 psi

@Temperature 2370 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.31 - 1.41 W/m-K

@Temperature 600 °C
9.09 - 9.79 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.35 - 1.45 W/m-K

@Temperature 100 °C
9.37 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.38 - 1.48 W/m-K

@Temperature 1300 °C
9.58 - 10.3 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
Shrinkage -0.300 - 0.300 %

@Temperature 1300 °C
-0.300 - 0.300 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 85 %
85 %
Fe2O3 1.0 %
1.0 %
SiO2 6.0 %
6.0 %
Descriptive Properties Value Comments
ASTM Classification F
Material Consumption per 1 m3 2550 kg