Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name GOLITE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 1.00 - 2.00 MPa

@Temperature 100 °C
145 - 290 psi

@Temperature 212 °F
Cold Crushing Strength
1.00 - 2.00 MPa

@Temperature 1000 °C
145 - 290 psi

@Temperature 1830 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.200 - 0.300 W/m-K

@Temperature 100 °C
1.39 - 2.08 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.240 - 0.340 W/m-K

@Temperature 600 °C
1.67 - 2.36 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.270 - 0.370 W/m-K

@Temperature 1000 °C
1.87 - 2.57 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1250 °C
2280 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1000 °C
-0.400 - 0.400 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 33 %
33 %
Fe2O3 1.0 %
1.0 %
SiO2 55 %
55 %
Descriptive Properties Value Comments
ASTM Classification Q
Material Consumption per 1 m3 830 kg