Material Notes:
Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 13.0 - 19.0 MPa

@Temperature 1370 °C
1890 - 2760 psi

@Temperature 2500 °F
Cold Crushing Strength
17.0 - 23.0 MPa

@Temperature 100 °C
2470 - 3340 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.350 - 0.450 W/m-K

@Temperature 100 °C
2.43 - 3.12 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.460 - 0.560 W/m-K

@Temperature 1370 °C
3.19 - 3.89 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Maximum Service Temperature, Air 1400 °C
2550 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1370 °C
-0.500 - 0.500 %

@Temperature 2500 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 45 %
45 %
Fe2O3 1.5 %
1.5 %
SiO2 41 %
41 %
Descriptive Properties Value Comments
ASTM Classification R
Material Consumption per 1 m3 1430 kg
Mixing Water 20-25 liters