Material Notes:
Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.50 - 1.60 g/cc
0.0542 - 0.0578 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 13.0 - 19.0 MPa

@Temperature 1260 °C
1890 - 2760 psi

@Temperature 2300 °F
Cold Crushing Strength
22.0 - 28.0 MPa

@Temperature 100 °C
3190 - 4060 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.360 - 0.460 W/m-K

@Temperature 100 °C
2.50 - 3.19 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.410 - 0.510 W/m-K

@Temperature 600 °C
2.85 - 3.54 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.470 - 0.570 W/m-K

@Temperature 1260 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 2300 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
Shrinkage -1.00 - 1.00 %

@Temperature 1260 °C
-1.00 - 1.00 %

@Temperature 2300 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 52 %
52 %
SiO2 40 %
40 %
Descriptive Properties Value Comments
ASTM Classification R
Material Consumption per 1 m3 1470 kg
Mixing Water 18-22 liters
per 100 kgs dry material