Material Notes:
Description: This type of brick, based on silicon carbide, is because of a very good thermal shock resistance, abrasion resistance and a high thermal conductivity very well suited for waste incinerator furnaces, aluminum furnaces, muffle furnaces and applications where a high abrasive resistance is requiredRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.55 g/cc
0.0921 lb/in³
Apparent
Porosity 16 %
16 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 150 MPa
21800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 6.50 W/m-K

@Temperature 1100 °C
45.1 BTU-in/hr-ft²-°F

@Temperature 2010 °F
7.10 W/m-K

@Temperature 650 °C
49.3 BTU-in/hr-ft²-°F

@Temperature 1200 °F
8.50 W/m-K

@Temperature 100 °C
59.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1550 °C
2820 °F
Deformation under load - t<sub>a</sub>
1550 °C
2820 °F
Component Elements Properties Metric English Comments
SiO2 70 %
70 %
Descriptive Properties Value Comments
Thermal Shock Resistance Min 30 cycles
DIN 51068