Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name VIBRON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack and abrasion in aluminum melting furnaces.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 95.0 - 105 MPa

@Temperature 1300 °C
13800 - 15200 psi

@Temperature 2370 °F
Cold Crushing Strength
105 - 115 MPa

@Temperature 100 °C
15200 - 16700 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.85 - 2.05 W/m-K

@Temperature 100 °C
12.8 - 14.2 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.85 - 2.05 W/m-K

@Temperature 600 °C
12.8 - 14.2 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.90 - 2.10 W/m-K

@Temperature 1300 °C
13.2 - 14.6 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1350 °C
2460 °F
Shrinkage -0.500 - 0.300 %

@Temperature 1300 °C
-0.500 - 0.300 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 73 %
73 %
Fe2O3 1.2 %
1.2 %
SiO2 11 %
11 %
ZrO2 6.0 %
6.0 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2900 kg
Mixing Water 4.5-5.5 liters
per 100 kgs dry material