Material Notes:
Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags. Due to special additions this material can be pumped and shotcreted.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.60 - 2.70 g/cc
0.0939 - 0.0975 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 75.0 - 85.0 MPa

@Temperature 100 °C
10900 - 12300 psi

@Temperature 212 °F
Cold Crushing Strength
90.0 - 110 MPa

@Temperature 1400 °C
13100 - 16000 psi

@Temperature 2550 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.25 - 1.35 W/m-K

@Temperature 100 °C
8.68 - 9.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.28 - 1.38 W/m-K

@Temperature 600 °C
8.88 - 9.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.50 - 1.70 W/m-K

@Temperature 1400 °C
10.4 - 11.8 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1400 °C
-0.500 - 0.500 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 73 %
73 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 26 %
26 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2600 kg
Mixing Water 5.5-6 liters
per 100 kgs dry material