Material Notes:
GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface identifiable, the laminate is branded with the GRAFOIL® grade and source guarantee. Grade GHR is suitable for standard industrial fluid sealing applications as well as applications in: chemical, petrochemical, refinery, steam service, cryogenic, and ASME class 150 & 300 flanges. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced. Laminate Construction: GRAFOIL® Grade GTB ? 0.002" thick flat 316 or 316L stainless steel (per ASTM F-A-240 and AMS 5524) ? GRAFOIL® Grade GTB
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
Thickness 810 microns
31.9 mil
Standard; Laminate
1570 microns
61.8 mil
Standard; Laminate
3100 microns
122 mil
Standard; Laminate
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.2 MPa
3800 psi
additive of steel and GRAFOIL® flexible graphite
Compression Set 85 %

@Pressure 34.5 MPa
85 %

@Pressure 5000 psi
after 5000 psi load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 525 °C
977 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Descriptive Properties Value Comments
"m" Factor 2
ASME Gasket Factor
"y" Stress (psi) 900
ASME Gasket Factor
Compressibility (%) 40
at 5000 psi load
Max Gasket Unit Load (psi) 24000
ASME Gasket Factor
Resistance in #1 Oil (%) <33
Weight change
<8
Thickness increase
Resistance in #3 Oil (%) <12
Thickness increase
<35
Weight change