Material Notes:
GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC can be used in a number of automotive or internal combustion applications. Additionally, GTC's ability to conform to less-than-ideally-finished surfaces is a benefit in aftermarket gasket applications. GTC is used in high-temperature sealing applications where binder-based materials fail. It is often combined with inserts to make head gaskets, exhaust manifold gaskets, EGR assemblies and filler material for heat shields. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced.
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Thickness 380 microns
15.0 mil
Standard
510 microns
20.1 mil
Standard
640 microns
25.2 mil
Standard
760 microns
29.9 mil
Standard
890 microns
35.0 mil
Standard
Ash 3.0 %
3.0 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.48 MPa
650 psi
Compression Set 87 %

@Pressure 34.5 MPa
87 %

@Pressure 5000 psi
after 5000 psi load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 450 °C
842 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Component Elements Properties Metric English Comments
Carbon, C 97 %
97 %
Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) <= 10 ppm
<= 10 ppm
Leachable
Descriptive Properties Value Comments
Compressibility (%) 43
at 5000 psi load