GrafTech GRAFOIL® TG679 Expanded Natural Graphite Powder

Category Carbon , Graphite
Manufacturer GrafTech International
Trade Name GRAFOIL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GrafTech GRAFOIL® TG679 Expanded Natural Graphite Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GRAFOIL® Grade TG679 is an expanded natural graphite powder with consistent purity and good lubrication properties. Typical applications include using the graphite powder as an electrically conductive additive or as a thermal transfer enhancement in plastics and foams or as a lubricant. GRAFOIL® Grade TG679 has Nano particle-like properties at the macro particle pricing level.
Physical Properties Metric English Comments
Density 0.0620 g/cc
0.00224 lb/in³
A.D. (Scott)
Moisture Absorption at Equilibrium 0.30 %
0.30 %
0.5% max
Particle Size 2.5 µm
2.5 µm
Typical Particle Thickness
Specific Surface Area 20 m²/g
20 m²/g
Ash 2.5 %
2.5 %
3.5% max
Component Elements Properties Metric English Comments
Aluminum, Al 0.10 %
0.10 %
Barium, Ba 0.00040 %
0.00040 %
Calcium, Ca 0.26 %
0.26 %
Chromium, Cr 0.00040 %
0.00040 %
Copper, Cu 0.00090 %
0.00090 %
Iron, Fe 0.21 %
0.21 %
Magnesium, Mg 0.16 %
0.16 %
Manganese, Mn 0.0016 %
0.0016 %
Molybdenum, Mo 0.0012 %
0.0012 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.050 %
0.050 %
Titanium, Ti 0.0070 %
0.0070 %
Vanadium, V 0.00050 %
0.00050 %