Material Notes:
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ material is offered in a variety of through thickness thermal conductivities, available in roll or die-cut form and can be laminated with plastics and adhesives. An economical thermal interface material, HITHERM™ products will not dry out and no outgassing occurs under vacuum conditions. The conformability of HITHERM™ materials optimizes thermal properties, ensures excellent contact, and is maintained for the life of the assembly. Typical applications include thermal interfaces, chip burn-in, chip testing fixtures, DC-to-DC converters, CPU modules, microprocessors, and hot and cold plates.
Physical Properties Metric English Comments
Thickness 508 microns
20.0 mil
Thermal Properties Metric English Comments
CTE, linear -0.400 µm/m-°C
-0.222 µin/in-°F
In-Plane
27.0 µm/m-°C
15.0 µin/in-°F
Through Thickness
Specific Heat Capacity 0.711 J/g-°C
0.170 BTU/lb-°F
Thermal Conductivity 6.00 W/m-K
41.6 BTU-in/hr-ft²-°F
Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar)
240 W/m-K
1670 BTU-in/hr-ft²-°F
In-Plane; Angstrom's Method
Maximum Service Temperature, Air 400 °C
752 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 0.00100 ohm-cm
0.00100 ohm-cm
In-Plane
1.50 ohm-cm
1.50 ohm-cm
Through Thickness