Material Notes:
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprietary manufacturing and machining processes to ensure that Arlons properties consistently outperform the competition.Greene, Tweed offers several different Arlon materials, and all provide high tensile strength and elongation properties, excellent shear strength and creep resistance, outstanding fatigue resistance, broad chemical and radiation resistance, and no susceptibility to hydrolysis (steam/hot water). Our engineers work one on one with customers to find the right solution for each specific application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
ASTM D2240
Tensile Strength at Break 96.5 MPa
14000 psi
ASTM D368
49.6 MPa

@Temperature 149 °C
7200 psi

@Temperature 300 °F
Tensile Strength, Yield 117 MPa
17000 psi
ASTM D638
Elongation at Break 14 %
14 %
ASTM D638
Tensile Modulus 4.48 GPa
650 ksi
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
27.6 MPa

@Temperature 260 °C
4000 psi

@Temperature 500 °F
110 MPa

@Temperature 149 °C
16000 psi

@Temperature 300 °F
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
3.63 GPa

@Temperature 149 °C
526 ksi

@Temperature 300 °F
Shear Strength 26.2 MPa

@Temperature 260 °C
3800 psi

@Temperature 500 °F
ASTM D732
55.2 MPa

@Temperature 149 °C
8000 psi

@Temperature 300 °F
ASTM D732
98.6 MPa

@Temperature 23.9 °C
14300 psi

@Temperature 75.0 °F
ASTM D732
Descriptive Properties Value Comments
Color Natural