Greene Tweed Avalon® 57 PTFE, Thermoset Resin Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Greene Tweed
Trade Name Avalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Avalon® 57 PTFE, Thermoset Resin Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.05 g/cc
2.05 g/cc
ASTM D792
Deformation 2.3 %
2.3 %
2000 psi 78°F; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D1457
Elongation at Break 300 %
300 %
ASTM D1457
Coefficient of Friction, Dynamic 0.13
0.13
33.3 psi @ 150 fpm
Coefficient of Friction, Static 0.060
0.060
33.3 psi
K (wear) Factor 4.43 x 10-8 mm³/N-M
2.20 x 10-10 in³-min/ft-lb-hr