Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Manufacturer Greene Tweed
Trade Name Avalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
ASTM D792
Deformation 1.2 %
1.2 %
2000 psi 78°F; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D1457
Elongation at Break 300 %
300 %
ASTM D1457
Shear Strength 10.3 MPa

@Temperature 204 °C
1500 psi

@Temperature 400 °F
ASTM D732
11.4 MPa

@Temperature 149 °C
1650 psi

@Temperature 300 °F
ASTM D732
12.4 MPa

@Temperature 93.3 °C
1800 psi

@Temperature 200 °F
ASTM D732
15.9 MPa

@Temperature 26.7 °C
2300 psi

@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Dynamic 0.12
0.12
33.3 psi @ 150 fpm
K (wear) Factor 2.01 x 10-8 mm³/N-M
1.00 x 10-10 in³-min/ft-lb-hr
Descriptive Properties Value Comments
Color Black