Material Notes:
Chemraz® 570, recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control is required, offers excellent performance in long-term static photolithography, acid/solvent and ultrapure H2O applicationsApplications:Valve sealsFitting and union sealsGasketsRegulator sealsFilter sealsDispensing sealsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D1414
Tensile Strength, Yield 2.41 MPa
350 psi
@50% Elongation; ASTM D1414
5.38 MPa
780 psi
@100% Elongation; ASTM D1414
Elongation at Break 145 %
145 %
ASTM D1414
Compression Set 35 %
35 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 210 °C
410 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color White