Greene Tweed CHEMRAZ® 605 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 605 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz® 605, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. A high temperature compound with superior compression set resistance, physical properties and excellent chemical resistance, it excels in demanding static and semi-dynamic applications. Chemraz 605 exhibits good performance with hot amines, steam and water and functions well in increased temperatures ranging from -4°F to 500°F (-20°C to 260°C).Available in O-rings, gaskets and many other custom shapes, Chemraz 605 possess a broad chemical resistance range. The 605 compound is suitable for use in a wide variety of media including acids, caustics, aldehydes, esters, ethers, aromatics, hot water, steam, amines, methanol, ketones, TBA ad MTBE.Applications:Mechanical sealsValvesPump HousingsSampling/metering equipmentCompressorsReactorsMixersControls/instrumentationSprayers/dispensersCouplingsDiaphramsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.97 g/cc
1.97 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 14.8 MPa
2150 psi
ASTM D1414
Tensile Strength, Yield 2.90 MPa
420 psi
@50% Elongation; ASTM D1414
9.03 MPa
1310 psi
@100% Elongation; ASTM D1414
Elongation at Break 130 %
130 %
ASTM D1414
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Descriptive Properties Value Comments
Color Black