Greene Tweed WRâ„¢ 575 PEEK, Bi-Directional Carbon Fiber Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Greene Tweed
Trade Name WR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed WRâ„¢ 575 PEEK, Bi-Directional Carbon Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material ideal for axial thrust and face loading applications. WR575 provides superior wear characteristics, enabling users to extend mean time between repairs.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 627 MPa
91000 psi
ASTM D3039
Tensile Modulus 60.0 GPa
8700 ksi
ASTM D3039
Flexural Strength 827 MPa
120000 psi
ASTM D790
Flexural Modulus 48.3 GPa
7000 ksi
ASTM D790
Compressive Strength 572 MPa
83000 psi
ASTM D695
Compressive Modulus 55.2 GPa
8000 ksi
ASTM D695
Descriptive Properties Value Comments
Color Black