Gwent Electronic Materials C2000802P2 Carbon Graphite Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2000802P2 Carbon Graphite Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is designed to be used for screen-printing working electrodes. This ink has been optimized to give superior electrochemical performance. It combines good line definition and good electrochemical performance with good reversibility when using cyclic voltammetery. This ink can be used in conjunction with UV dielectrics and ink is fast drying for slower drying please see C2030519P4. Screen Printing Equipment: automatic, semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-230tpiSubstrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 39 - 41 %

@Temperature 130 °C
39 - 41 %

@Temperature 266 °F
Viscosity 2000 - 3500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
2000 - 3500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 10.0 microns
0.394 mil
Cured, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 100 ohm
100 ohm
Typical, Printed through 230 stainless steel mesh with 13 micron emulsion
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 80.0 °C
0.250 hour

@Temperature 176 °F
30.0 min

@Temperature 30.0 °C
0.500 hour

@Temperature 86.0 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 305
Using a 230 mesh stainless steel screen