Gwent Electronic Materials D2080121D12 Dielectric Ink

Category Fluid , Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials D2080121D12 Dielectric Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is a thermoplastic screen printing ink, developed for use for flexible polymer applications. It is printed on to flexible polymeric substrates, such as Polyimide and PET substrates, to create an insulation layer over highly conductive tracks for general circuit applications. It is compatible with a range of silver and carbon curing systems in order to construct simple circuits. The ink has under gone extensive electrical and mechanical testing to show that it is very flexible. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156 to 325tpiSubstrate: Polyester, PVC, or CeramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 47 - 48 %

@Temperature 150 °C
47 - 48 %

@Temperature 302 °F
for 60 min
Viscosity 9500 - 14000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
9500 - 14000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 150 °C
0.250 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 260
Using a 230 mesh stainless steel screen