Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

H.C. Starck Amperit® 583.054 Chromium Carbide-Nickel 83-17 (Cr3C2-Ni)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 583.054 Chromium Carbide-Nickel 83-17 (Cr3C2-Ni).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 2.50 - 3.30 g/cc
0.0903 - 0.119 lb/in³
ASTM B212
Particle Size 14 - 20 µm
14 - 20 µm
10%
31 - 37 µm
31 - 37 µm
50%
53 - 62 µm
53 - 62 µm
90%
Component Elements Properties Metric English Comments
Carbon, C 10 - 11.5 %
10 - 11.5 %
Iron, Fe <= 0.50 %
<= 0.50 %
Nickel, Ni 16 - 18 %
16 - 18 %