Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hannam Chemical Hanalac 750 ABS, General Purpose

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Hannam Chemical
Trade Name Hanalac
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hannam Chemical Hanalac 750 ABS, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: electronic home appliances (TVs, fans, mixers, switch panels), calculators and cash registers, telephones.
Physical Properties Metric English Comments
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 64.0 MPa
9280 psi
ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Notched 2.50 J/cm

@Thickness 3.17 mm
4.68 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Flammability, UL94 HB
HB