Material Notes:
The 14100 series bulk molding compound is an electrical grade material that can be compression, transfer, or injection molded. Offering good mechanical strength and excellent electrical properties, this grade also exhibits low shrink characteristics. The 14100 BMC is recognized by UL with a 94V-0 flame rating at .060" wall thickness.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
ASTM D572
Water Absorption 0.10 %
0.10 %
ASTM D570
Linear Mold Shrinkage 0.00075 cm/cm
0.00075 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
Flexural Strength 86.0 MPa
12500 psi
Compressive Strength 90.0 MPa
13100 psi
Izod Impact, Notched 1.90 J/cm
3.56 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Flammability, UL94 V-0
V-0
File No.E-27875
Electrical Properties Metric English Comments
Dielectric Constant 5.0

@Frequency 60 Hz
5.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
Perpendicular (ASTM D149), Short Time
Dissipation Factor 0.033

@Frequency 60 Hz
0.033

@Frequency 60 Hz
ASTM D150
Arc Resistance 192 sec
192 sec
ASTM D495
Comparative Tracking Index 600 V
600 V