Haysite 18600 Polyester BMC, 15% Glass Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Haysite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite 18600 Polyester BMC, 15% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 18600 series bulk molding compound can be compression, transfer, or injection molded. Formulated with a high temperature resin system, this grade exhibits exceptional retention of physical and electrical properties after exposure to elevated temperatures.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
ASTM D572
Water Absorption 0.11 %
0.11 %
ASTM D570
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.0 MPa
6240 psi
Flexural Strength 97.0 MPa
14100 psi
Compressive Strength 103 MPa
14900 psi
Izod Impact, Notched 2.10 J/cm
3.93 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Constant 8.5

@Frequency 60 Hz
8.5

@Frequency 60 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
Perpendicular (ASTM D149), Short Time
Dissipation Factor 0.067

@Frequency 60 Hz
0.067

@Frequency 60 Hz
ASTM D150
Arc Resistance 188 sec
188 sec
ASTM D495