Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Haysite 46000 Polyester SMC, 30% Glass Reinforced

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Haysite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite 46000 Polyester SMC, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 46000 series sheet molding compound is designed for "automotive type" applications requiring good mechanical properties and low shrink characteristics.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D572
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.00070 cm/cm
0.00070 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 83.0 MPa
12000 psi
Flexural Strength 207 MPa
30000 psi
Compressive Strength 193 MPa
28000 psi
Izod Impact, Notched 9.90 J/cm
18.5 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Constant 4.9

@Frequency 60 Hz
4.9

@Frequency 60 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
Perpendicular (ASTM D149), Short Time
Dissipation Factor 0.0060

@Frequency 60 Hz
0.0060

@Frequency 60 Hz
ASTM D150
Arc Resistance 140 sec
140 sec
ASTM D495