Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant

Category Polymer , Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HCR-125 is a corrosion resistant vinyl ester sheet created by impregnating fiber glass mat, synthetic surface veil, and inert additives with Derkane 470 resin and catalyst. A compression molded product is produced by controlling a chemical reaction under heat and extreme pressure. Haysite HCR-125 offers excellent strength to weight ratios in addition to their corrosion resistance. Application: HCR-125 material can be sawed, sheared, machined, and punched to any size and shape. Successful applications include: tanks, tank covers, ductwork, exhaust and fume hoods, separators, bins, fan housings, trays, hoppers, sinks, lab table tops, fume scrubbers, heat exchanger plates, filter press plates, and other applications requiring a material with excellent resistance to corrosive elements. Standard color - Beige.Information provided by Haysite
Physical Properties Metric English Comments
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 54
54
Tensile Strength 74.5 MPa
10800 psi
ASTM D638
Flexural Strength 167.0 MPa
24220 psi
ASTM D790
Compressive Strength 241 MPa
35000 psi
ASTM D695
Shear Strength 96.5 MPa
14000 psi
ASTM D732
Izod Impact, Notched 5.13 J/cm
9.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 13.8 kV/mm
350 kV/in
Perpendicular in Oil; ASTM D149
Dielectric Breakdown 64000 V
64000 V
Parallel, in Oil; ASTM D149
Arc Resistance 191 sec
191 sec
ASTM D495
Descriptive Properties Value Comments
Flame Resistance 113 seconds
Ignition Time, ASTM D229
45 seconds
Burning Time, ASTM D229