Material Notes:
A special blend of graphites suited for cover on neutral salts especially for use with Nu-SalInformation provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1200 °C
2200 °F
Upper limit of working range
Minimum Service Temperature, Air 760 °C
1400 °F
Lower limit of working range