Heatbath/Park Low Temperature Draw Salt Quenching and Tempering Salt

Category Ceramic , Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park Low Temperature Draw Salt Quenching and Tempering Salt.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A eutectic mixture offering the lowest melting point and a wide working range. Formulated per MIL-S-10699-B, Class 1 (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
Maximum Service Temperature, Air 593 °C
1100 °F
Upper limit of working range
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range