Heatbath/Park Pen Kase 5 Carburizer

Category Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park Pen Kase 5 Carburizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cyanide Liquid Carburizer. Water-soluble liquid carburizing salt offering easy cleaning, good fluidity and high stability. Will produce carbonitrided cases in lower temperature ranges and carbon cases in higher temperature ranges, usually up to about 0.050 inches.Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 566 °C
1050 °F
Maximum Service Temperature, Air 954 °C
1750 °F
Upper limit of working range
Minimum Service Temperature, Air 621 °C
1150 °F
Lower limit of working range