Henkel Bonderite 7400 Conversion Coating

Category Fluid , Solvent
Manufacturer Henkel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Bonderite 7400 Conversion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bonderite 7400 is formulated for non-rinsing, dry-in-place that produces a uniform conversion coating, which improves adhesion and bare corrosion resistance on aluminum, galvanized steel, iron, steel and zinc surfaces.
Descriptive Properties Value Comments
Chemistry Non-chrome
Consistency Liquid
Form Concentrated
Substrate Aluminum
Ferrous