Material Notes:
One-part Infusion resin for RTM & VARTM processing. Low viscosity, high hot-wet properties and very good resistance against flame, smoke and toxicity.
Physical Properties Metric English Comments
Storage Temperature 23.0 °C
73.4 °F
Mechanical Properties Metric English Comments
Tensile Strength 71.0 MPa
10300 psi
Elongation at Break 1.5 %
1.5 %
Tensile Modulus 0.00440 GPa
0.638 ksi
Flexural Modulus 0.00450 GPa

@Temperature 25.0 °C
0.653 ksi

@Temperature 77.0 °F
Flexural Stiffness 161 MPa

@Temperature 25.0 °C
23400 psi

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Processing Properties Metric English Comments
Cure Time 90.0 min

@Temperature 180 °C
1.50 hour

@Temperature 356 °F
Descriptive Properties Value Comments
Consistency Low Viscosity
Form 1 part
Fracture Toughness (J/m2) 112
Pot Life 6 months