Material Notes:
Excellent peel and shear strength. Bonds a variety of substrates.Applications: Structural Repair Composite Bonding
Physical Properties Metric English Comments
Storage Temperature 25.0 °C
77.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 36.6 MPa
5310 psi
Elongation at Break 7.7 %
7.7 %
Tensile Modulus 2.20 GPa
319 ksi
Adhesive Bond Strength 6.90 MPa

@Temperature 93.0 °C
1000 psi

@Temperature 199 °F
Tensile Lap Shear
27.6 MPa

@Temperature -55.0 °C
4000 psi

@Temperature -67.0 °F
Tensile Lap Shear
31.0 MPa

@Temperature 25.0 °C
4500 psi

@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 13.4 kN/m
76.5 pli
Bell Peel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 82.0 °C
1.00 hour

@Temperature 180 °F
7200 - 10100 min

@Temperature 25.0 °C
120 - 168 hour

@Temperature 77.0 °F
Pot Life 40 min
40 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 100:44
Peel Strength High