Moldable plastic shim, excellent microcracking resistance under thermal cycling. High compressive strength.Application: Liquid Shim
Physical Properties Metric English Comments
Storage Temperature 4.00 °C
39.2 °F
Mechanical Properties Metric English Comments
Compressive Strength 110.3 MPa
16000 psi
Compressive Modulus 4.82 GPa
699 ksi
Adhesive Bond Strength 13.8 MPa

@Temperature 93.0 °C
2000 psi

@Temperature 199 °F
Tensile Lap Shear
15.9 MPa

@Temperature -55.0 °C
2310 psi

@Temperature -67.0 °F
Tensile Lap Shear
15.9 MPa

@Temperature 25.0 °C
2310 psi

@Temperature 77.0 °F
Tensile Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 93.0 °C
>= 199 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 82.0 °C
1.00 hour

@Temperature 180 °F
7200 - 10100 min

@Temperature 25.0 °C
120 - 168 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 100:19
Peel Strength Nil