Material Notes:
Low-density, one-component epoxy syntactic for use on honeycomb composite parts requiring high compressive strength at temperatures up to 350°F / 177°C. Ideal for fastener or attachment potting and panel edge reinforcing.Applications: Potting Syntactic
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Compressive Strength 84.0 MPa
12200 psi
Adhesive Bond Strength 14.0 MPa

@Temperature 25.0 °C
2030 psi

@Temperature 77.0 °F
Tensile Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 171 °C
1.00 hour

@Temperature 340 °F
90.0 min

@Temperature 121 °C
1.50 hour

@Temperature 250 °F
Pot Life 480 min
480 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 1 part
Peel Strength Nil