Material Notes:
Tougher version of Hysol PL 795. Excellent flow characteristics. Excellent tack and handling characteristics. Improved elevated temperature performance. Can be used for both surfacing film and lightning strike applications.Applications: Composite Bonding Composite Surfacing
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 6.90 MPa
1000 psi
Flatwise
Adhesive Bond Strength 13.1 MPa

@Temperature 149 °C
1900 psi

@Temperature 300 °F
Lap Shear
24.8 MPa

@Temperature -55.0 °C
3600 psi

@Temperature -67.0 °F
Lap Shear
29.7 MPa

@Temperature 25.0 °C
4310 psi

@Temperature 77.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 177 °C
1.00 hour

@Temperature 351 °F
90.0 min

@Temperature 121 °C
1.50 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Out-Time (days) 100
at 25°C