Material Notes:
Turco 5351 (T-5469) is a yellow, viscous paint remover developed to remove epoxy, polyurethane and similar coatings from metal surfaces at ambient temperatures. Turco 5351 (T-5469) clings to vertical and overhead surfaces and forms a surface film that helps retard evaporation and extend the working life of the stripper. Turco 5351 (T-5469) should not be used on material that are affected by chlorinated hydrocarbons.
Processing Properties Metric English Comments
Processing Temperature 23.0 °C
73.4 °F
Descriptive Properties Value Comments
Chemistry Neutral methylene chloride based
Consistency Liquid
Form Ready-to-Use
Substrate Aluminum
Ferrous
Magnesium
Non-Ferrous
Stainless Steel
Titanium