Material Notes:
Turco Aluminux Etch L is a concentrated liquid alkaline product developed to produce a fine satin etch on aluminum and its alloys. It offers an exceptionally uniform etch and extended bath life.Applications:Alkaline EtchConversion CoatingsBoric Sulfuric AnodizingChromic Acid Anodizing
Descriptive Properties Value Comments
Chemistry Strong Alkaline
Consistency Liquid
Form Concentrated
Substrate Aluminum