Henkel Turco Liquid Sprayeze NP-LT Cleaner

Category Fluid , Solvent
Manufacturer Henkel
Trade Name Turco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Turco Liquid Sprayeze NP-LT Cleaner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Turco Liquid Sprayeze NP-LT is a straw-colored liquid, developed to remove shop soil, lube oils, light drawing oils and drawing waxes from ferrous, aluminum, copper and titanium alloys. In addition, it is also suitable for cleaning most magnesium alloys, zinc and cadmium, and is ideal for precleaning metals prior to phosphating and painting.Applications:Aqueous DegreasingAlkaline EtchConversion CoatingsBoric Sulfuric Anodizing Chromic Acid Anodizing Phosphoric Acid Anodizing
Processing Properties Metric English Comments
Processing Temperature 38.0 - 60.0 °C

@Time 900 sec
100 - 140 °F

@Time 0.250 hour
Immersion
Descriptive Properties Value Comments
Chemistry Alkaline
Water-based
Consistency Liquid
Form Concentrated
Substrate Aluminum
Ferrous
Magnesium
Stainless Steel
Titanium