Material Notes:
Hexcel features custom fabric design and manufacturing. We tailor our customers' reinforcement fabrics for optimum performance. We are able to combine two or more different fibers (carbon, glass, aramid, ceramics, Thorstrand™), to use different weaving solutions, produce preforms, etc.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 201 microns
7.90 mil
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 5
Dry
Nominal Construction (count/in) 16
Warp
16
Fill
Type of Yarn Fill Yarn: ECG 75 1/0
Warp Yarn: 3K Carbon, 33 MSI
Weave Style Plain